1. Occasionally, a bubble is not removed during refining, a sand grain refuses to melt, a tremor in the tin puts ripples into the glass ribbon.
"有时候,在提炼的过程中会出现这些情况:一个气泡没有被移除,一个砂粒没有熔化,(熔融的)锡的一次颤动把波纹带进了玻璃带中。

youdao

2. When pouring molten glass onto the molten tin, the underside of the glass would also be perfectly flat.
当把玻璃液倒在锡液上时,玻璃的底面也会变得完全平整。

youdao

3. The glass settled to a thickness of six millimetres because of surface tension interactions between the glass and the tin.
由于玻璃和锡之间的表面张力的相互作用,玻璃的厚度降到了6毫米。

youdao

4. If the glass were kept hot enough, it would flow over the molten tin until the top surface was also flat, horizontal and perfectly parallel to the bottom surface.
如果玻璃保持足够的温度,它就会在熔化的锡中流动,直到顶部表面也变得平整、水平,与底部表面完全平行。

youdao

5. It was fashioned from a lunch box, camera, opera glass parts, pie servers, springs, gooseneck lamp part, drapery rod finial, clock key, and tin cups.
这是从一个饭盒,老式相机,歌剧玻璃零件,馅饼服务器,弹簧,鹅颈灯的一部分,布料杆顶尖,时钟键,锡杯。

youdao

6. Tin bath is the equipment for glass forming in float process.
锡槽是浮法玻璃工艺中的成型设备。

youdao

7. Yes. You should take your glass, paper, plastic, cardboard, and tin cans to a recycling center.
有的。玻璃,纸张,塑料,硬板纸盒,罐头盒都可以送进回收中心。

youdao

8. This article also describes some efficient steps for operating edge roller , stabilizing convection of tin fluid and settling flow of glass fluid .
本文将从合理使用拉边机、稳定锡液对流、稳定玻璃液流等方面所采取的有效措施作一些介绍。

youdao

9. Tin doped indium oxide (ITO) films were deposited on glass substrates by reactive magnetron sputtering using a metallic alloy target (in Sn, 90 10).
采用铟锡合金靶(铟锡,90 - 10),通过直流反应磁控溅射在玻璃基片上制备出ito薄膜,并在大气环境下高温退火处理。

youdao

10. The problem of phase separation in lead tin fluorophosphate glass had been solved, and a relatively stable glass compositions had been designed.
解决了铅锡氟磷酸盐玻璃中存在的分相问题,设计了较好的玻璃组分。

youdao

11. The optical interference layers are deposited between the glass substrate and ITO(indium tin oxide) anode, which could partly suppress the reflection of ambient light.
在玻璃衬底和ITO阳极之间溅射的光学干涉层可以部分消去背景光的反射。

youdao

12. It is shown by the diagnosis of tin surface layer that the dielectric constant in the tin surface layer is larger than that inside the float glass.
渗锡层诊断证明:渗锡层的介电常数大于浮法玻璃内部的介电常数。

youdao

13. For excellent float glass product view points of authors on formula, raw materials, melting, tin bath and control way were put forwarded.
为打造浮法精品,从配方、原料、熔化、锡退及控制方法等方面提出自己的观点。

youdao

14. Stout is a key place which joins furnace with tin slot. It mainly includes stout brick and lip brick. The lip brick's quality directly influences the glass 'yield and quality.
流槽是连接熔窑和锡槽的一个关键部位,主要包括流槽砖和唇砖,其中唇砖的好坏直接影响玻璃的产、质量。

youdao

15. A pretreatment process before the surface of the glass fiber is plated with tin and nickel mainly comprises the following steps of: deoiling, coarsening, sensibilizing, activating, and the like.
玻璃纤维表面化学镀锡镍前的预处理工艺主要包括除油、粗化、敏化、活化等。

youdao

16. The principle of intelligent power con - troller and its application to float glass line were introduced and the use of intelligent optimum pow - er splitting in heating control of tin bath.
介绍了智能调功器的原理及其在浮法玻璃生产线上的实际应用情况,并重点指出了智能优化功率分配在锡槽加热控制中的应用。

youdao

17. RPC Corby sales and marketing manager Vince Dean said the firm's handling, filling and decoration facilities made the Classic jar a "genuine alternative to glass and tin".
科比的RPC的销售和营销经理文院长说,该公司的处理,灌装及装修设施经典罐子“真正替代玻璃和锡。”

youdao

18. Foreign substances which have adhered to a glass ribbon, such as tin and tin oxide, are removed during glass sheet production.
本发明是在玻璃片材的制造中除去附着于玻璃带的锡和氧化锡等异物。

youdao

19. This machine was made to seal not only the glass bottles but also the tin-plate cans.
通过增加一个气筒和延时装置,使之不仅可用于玻璃瓶封口,而且可用于金属罐封口。

youdao

20. Zinc oxide thin films were prepared by pulsed laser deposition (PLD) on glass substrates coated with tin-doped indium oxide (ITO) thin films in this paper.
本文采用射频辅助脉冲激光沉积(PLD)系统,在镀有透明导电膜氧化锡铟(ito)的玻璃衬底上制备了氧化锌薄膜。

youdao

21. It had a BZE39 or BZ40 fitted on a threaded tin cover which bayonet-fitted the glass collar.
它有一个BZE39或BZ 40线程上的刺刀锡盖,装上玻璃衣领装置。

youdao

22. Next in a mixing tin muddle 4 fresh raspberries, 1 1/4oz chilled TIO PEPE XERES and 3/4oz Monin Raspberry Syrup. Add ice. Shake and strain into a urban bar glass.
然后,在一个混合波士顿摇壶中混合4个新鲜树莓,1 1/4盎司冰鲜干雪利酒和3/4盎司小红莓糖浆,加入冰,摇晃后倒入一个城市酒吧杯中。

youdao

23. The foreground of applying indium tin oxide film to heat-insulating and energy \ | saving in glass field has been analysed.
分析了氧化铟锡薄膜应用于玻璃领域隔热节能的前景。

youdao

24. The Indium-tin oxide (ITO) films were prepared on glass substrate using sol-gel dip coating method.
采用溶胶-凝胶工艺,用提拉法在玻璃基底上制备了ITO透明导电薄膜。

youdao

25. The Indium-tin oxide (ITO) films were prepared on glass substrate using sol-gel dip coating method.
采用溶胶-凝胶工艺,用提拉法在玻璃基底上制备了ITO透明导电薄膜。